| Test method | Property | Result | SATRA recommended value |
| Satra PM94: 1993* |
Breaking load ( N ) | Dry : 354 Wet : 428 |
200 min 150 min |
| Satra PM93: 1993* |
Lace to eyelet abrasion ( Number of cycles to failure ) |
All samples : > 5.000 abrasion cycles with no failure |
> 5.000 cycles with no failure
|
| Satra PM154: 1992* |
Lace to lace abrasion ( number of cycles to failure ) |
All samples : > 5.000 abrasion cycles with no failure |
> 5.000 cycles with no failure |
| Satra PM195D : 1996 |
Resistance to knot slippage ( N ) |
52 | 30 min |